Dense nanocrystalline W alloys: Enhancement of hardness and thermal stability by Al addition

Torre, Francesco;Barra, Paolo;Delogu, Francesco;Orru, Roberto;Cao, Giacomo;Locci, Antonio Mario
2023-01-01

Abstract

Nanocrystalline W100-xAlx (x up to 20 at.%) powders obtained by mechanical alloying have been consolidated by spark plasma sintering (SPS). Alloying W with Al significantly improves the sinterability, allowing the fabrication of dense samples. The consolidation process keeps the nanocrystalline microstructure substantially unaffected, which contributes to the hardness of the final W-Al alloys. The room-temperature nano-and micro-hardness of dense W80Al20 alloy sintered at 1100 degrees C are as high as 18 and 14 GPa, respectively. These values are significantly higher than those previously reported for pure coarse-or submicron-grained W and may be ultimately ascribed to the grain boundary segregation of Al.
2023
Inglese
112
106150
12
Esperti anonimi
scientifica
Spark plasma sintering; Nanocrystalline; W alloys; Al alloys; Hardness
Torre, Francesco; Huminiuc, Theodor; Barra, Paolo; Pilloni, Luciano; Polcar, Tomas; Rinaldi, Antonio; Delogu, Francesco; Orru, Roberto; Cao, Giacomo; ...espandi
1.1 Articolo in rivista
info:eu-repo/semantics/article
1 Contributo su Rivista::1.1 Articolo in rivista
262
10
open
File in questo prodotto:
File Dimensione Formato  
1-s2.0-S0263436823000501-main_compressed.pdf

accesso aperto

Tipologia: versione editoriale
Dimensione 960.28 kB
Formato Adobe PDF
960.28 kB Adobe PDF Visualizza/Apri

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Questionario e social

Condividi su:
Impostazioni cookie